J-R fracture resistance, dynamic strain aging (DSA), SA516-Gr.70 steel, loading rate, LBB INTRODUCTION SA516-Gr.70 steel has been widely used for elbows of nuclear piping. The leak-before-break (LBB) design concept [1] that has been applied to nuclear piping recently requires confirming fracture resistance of the piping materials through J-R tests. However, the systematic J-R test data obtained under various test conditions are very rare while a large database has been built for another piping material, i.e. SA106 steel by the International Piping Integrity Research Group (IPIRG) program. It is well known that the fracture resistances of ferritic steels like SA516-Gr.70 steel are deteriorated in dynamic strain aging (DSA) region. Although some researchers like Miglin et al. and Marengo et al. reported DSA effect in J-R fracture resistance [2,3], their investigations were limited to J-R tests under static loading condition. Therefore, J-R fracture resistances were investigated in the present study at various temperatures ranging from ambient to maximum reactor operating temperature and various loading rates for SA516-Gr.70 steels. DSA effects in of J-R fracture resistances of two heats of SA516-Gr.70 steels with loading rates and temperatures were analyzed. Furthermore, differences of DSA behaviors and fracture resistances between two test materials of same specification were described and discussed with respect to microstructure and chemical composition. EXPERIMENTAL Materials and Specimen Two heats of SA516-Gr.70 steels for elbow are used in this study. The chemical compositions are shown in Table 1. The ASTM standard 1T-C(T) specimens with T-L orientation were used for J-R tests. The specimens were side-grooved to a depth of 10% of the specimen thickness on both sides after fatigue pre-cracking. TABLE 1 CHEMICAL COMPOSITIONS OF SA516-Gr.70 STEELS wt.% Material C Si Mn P S Cu N Ni Cr Mo Al V Nb Mat. A 0.22 0.31 1.14 0.005 0.002 0.10 0.0088 0.21 0.15 0.04 0.020 <0.005 <0.05 Mat. B 0.17 0.30 1.14 0.009 0.001 0.20 0.0024 0.36 0.03 0.10 0.031 0.028 0.016 J-R fracture resistance test - 2 -

RkJQdWJsaXNoZXIy MjM0NDE=