ICF10B

1. INTRODUCTION Corrosion of implant metal is detrimental for two reasons. First, corrosion fatigue is a major risk factor in fracture of implant metals [1]. Second, released metallic ions may be toxic [2]. Therefore, corrosion of implant alloys is a serious problem. Not only simple corrosion behavior but also corrosion behavior with applied stress must be clarified because implant metals are often used under stress in vivo. In recent years, titanium alloys have been widely used as biomaterials. Although the effects of cyclic load on corrosion behaviors of titanium alloys have been reported [3], no detail work has focused on the effects of static stress on its’ corrosion behavior [4]. In the present study, to clarify the effects, anodic polarization tests were carried out in constant stress condition. 2. EXPERIMENTAL 2.1. Materials A β rich, α+β type titanium alloy (Ti-4.5Al-3V-2Mo-2Fe; with the commercial name of SP-700) was used. This alloy was annealed at 800°C for 8 hours. The configuration of the test specimens is shown in Figure 1. The surfaces of the specimens were ground and polished electrolytically. To avoid preferential corrosion of edges, the specimens were covered with inert coatings, leaving an exposed surface area of 1 cm2 (Figure 1). Figure 1: Configuration of the specimen 3 6 8 M14x1 R6 R30 12.5 4 16 2 R13 23 100 2.2. Corrosion test Figure 2 shows the schematic of the corrosion test system; a platinum auxiliary electrode and an Ag/AgCl reference electrode were used. A Ringer’s solution, a simulated physiological solution was used as the electrolyte. This solution was kept at a temperature of 37°C and was exposed to the atmosphere. Fist, a specimen was mounted on a polarization cell and on the chuck of a servohydraulic test system. Then static stress was applied using the servohydraulic test system followed by filling the polarization cell with the solution. Cyclic, anodic, potentiodynamic polarization tests were carried out with an automatic polarization system. The open-circuit potential, i.e., the corrosion potential, was recorded after maintaining constant stress for 30 min. The potential was potentiostatically kept to the measured corrosion potential for 1 hour then scanned anodically at a scan rate of 0.167 mV/s, from the corrosion potential, up to the potential of 4.0 V higher than the corrosion potential. Then the potential was scanned in the cathodic direction at the same scan rate until the applied potential reached the corrosion potential. Such anodic polarization tests were conducted

RkJQdWJsaXNoZXIy MjM0NDE=