Figure 5 compares the traction-free zone lengths and the total lengths of cohesive cracks in various metals. The lengths of elastic cracks are also plotted in the figure. All lengths are plotted against the cohesive strengths sc = 2g/ cr = g/b of the metals. In all cases, w = 1 o and 2a = 4 nm. The results show that the various lengths do not have a clear correlation with sc. Similarly, no clear correlation is found when they are plotted against g, G or KIC. In contrast, the length of an elastic Zener crack subjected to the opening bT (no disclination loading) varies monotonically with the material parameters. The figure also shows that the predicted length of a disclinated elastic crack overestimates the traction-free zone length of the cohesive crack but underestimates the total length of the cohesive crack. 4. SUMMARY The equilibrium length of a stable mode I Zener-Barenblatt crack subjected to the loading of a disclination dipole is investigated in this paper. The crack length solutions are obtained by the method of dislocation modeling of the entire cohesive crack. Exact expressions constructed from the crack opening displacement and the consistency relations are solved numerically for the total crack length and the cohesive zone lengths. For small crack head opening displacement of the order of nanometers, numerical results indicate that: (i) the cohesive zones constitute a significant portion of the total crack, (ii) the elastic crack length, while significantly larger than the traction-free zone length, is significantly smaller than the total cohesive crack length, (iii) the traction-free zone length increases with the disclination dipole strength and the dipole arm length, and (iv) the cohesive zone at the crack head decreases in size with the disclination parameters, while that at the crack tip increases in size with these parameters. REFERENCES 1. Mu&&llner, P. and Kuschke, W.-M. (1997). Scrip. Mater. 36, 1451. 2. Mu&&llner, P. (1997). Mater. Sci. Engng. A234-236, 94. 3. Wu, M. S. (2001). Int. J. Engng. Sci., accepted. 4. Pearson, W. B. (1967). Handbook of Lattice Spacings and Structures of Metals, Vol. 2. Pergammon Press, Oxford. 5. Hirth, J. (1982). Theory of Dislocations, Second Edition. Krieger Publishing Company, Malabar. Figure 5: Comparison of the total crack lengths (pentagons), the traction-free zone lengths (triangles) of cohesive cracks, and the crack lengths (crosses) of elastic cracks. Cohesive Strength, c (GPa) Length (nm) 2c – l1 – l2, cohesive 2c, cohesive 2c, elastic Al Ag Cu Fe Ni W
RkJQdWJsaXNoZXIy MjM0NDE=