ICF10B

Figure 8 shows the modified curve that was based on Eqn.5 for Figure 5. The fatigue limit was estimated as 385MPa from Figure 8, and this value agrees well with the experimental value of 370MPa. In the other materials which authors have used in a series of research as the SP-treated Type 316L, the HSP-treated Type 316 and the HSP treated Type 304 etc., sufficient estimation results were obtained with the accuracy of 10% [10-13]. Using Modified Goodman diagram In this paragraph, the estimation by using the modified Goodman’s diagram as Eqn.1-b is investigated. Since the tensile strength σB is depended on the hardness of matrix, relationship between the hardness and the tensile strength must be investigated of the Type 316L steel if the fatigue limit estimate by using the modified Goodman’s diagram. In this study, the tensile test using pre-strain specimen was carried out. As a result, next equation was obtained. [MPa] (6) Hv B 356 1.378 = + σ The fatigue limit was estimated by using the Eqn.1-b as modified Goodman’s diagram, Eqn.6 and the coefficient ratio Csurf/Cin as Eqn.5. As a result of this method, like the estimation using endurance fatigue limit, the fatigue limit of HSP-treated Type 316L was also estimated about 385MPa. CONCLUSION In order to estimate the rotating bending fatigue limit of the hard shot peening (HSP) treated Type 316L stainless steel, the method using the fatigue limit diagram, was applied. In this paper, it was clarified that there was the necessity to reconsider on these methods, and the new method to modified using the coefficient of equation to calculate the stress intensity factor was proposed. As a result of the investigation based on this modified method, the fatigue limit of HSP treated specimens was well estimated for the experimental values. References 1. Mitsubayashi,M., Miyata,R. and Aihara,H. (1995). Jpn. Soc. Mech. Eng.Ser.A, 61, 1172. 2. Ohuchida,H., Nishioka,A., and Hayama,T. (1972). Jpn. Soc. Mater. Sci. 21,733. 3. Horikawa,T., Nakamura,H., Kawamura,M., Kawasaki,K. and Misaka,Y. (1997). Jpn. Soc. Mater. Sci. 46,1242. 4. Murakami,M., Konbayashi,M., Makino,Y., Toriyama,H., Kurihara,Y., Takasaki,S. and Ebara,R. (1994).Trans. of JSSR,7 5. Nakamura,H.,Tsunenari,T.,Horikawa,T. and Okazaki,S.(1983). Fatigue Life Design of Machine, Yokendo.Ltd,Japan. 6. Tanaka,T. (1983). Reference of Fatigue Reliability Design on Metal. 7. Murakami,Y., (1987). Stress Intensity Factors Hand book Vol.3, Pergamon Press. 8. Murakami,Y., (1993). Metal Fatigue: Effects of Small Defects and Nonmetallic Inclusions, Yokendo.Ltd 9. Larsson, M., Melander, A., Blom,R. and Preston, S. (1991). Mater. Sci. Tech. 7,11,998 10. Masaki,K., Ochi, Y.and Ishii,A.,Mater. Sci. Res.Int.Vol.4,1998,pp.200-205. 11. Masaki,K., Thoumyou,.H, Ochi,Y. and Matsumura, T., . (1999). Jpn. Soc. Mech. Eng.Ser.A, 65, 334. 12. Masaki,K., Ochi,Y. and Matsumura, T., . (1999). Jpn. Soc. Mater. Sci. 48,1124. 13. Ochi,Y., Akashi,A., Masaki, K., and Matsumura, T., . (2000). Jpn. Soc. Mech. Eng.Ser.A, 66, 320.

RkJQdWJsaXNoZXIy MjM0NDE=