EVALUATION OF A BRITTLE FRACTURE ACCIDENT THAT OCCURRED AT THE HYOGO-KEN NANBU EARTHQUAKE M. TOYOSADA, K. GOTOH, Y. WATANABE and S. NAKAYAMA Department of Marine Systems Engineering, Kyushu University, Hakozaki 6-10-1, Higashi-ku Fukuoka, 812-8581, Japan ABSTRACT Many fracture accidents of steel structures, which did not enable to occur under static loading, were found at the Hyogo-ken Nanbu Earthquake (17 January, 1995). Considering the strain rate effect on fracture toughness was required to evaluate these fracture accidents quantitatively. The evaluation concept of fracture toughness at arbitrary strain rate is explained briefly. An analysis on the brittle fracture accident of centrifugal cast steel bridge pier for railway was performed by means of this method. The result makes clear that vertical impulsive seismic wave is considered to be the major cause of the brittle fracture accident generated on this bridge pier at the Hyogo-ken Nanbu Earthquake. KEYWORDS brittle fracture, strain rate, impulsive seismic wave, dynamic loading, Rprameter, cast steel bridge pier, Hyogo-ken Nanbu Earthquake INTRODUCTION Many fracture accidents of steel structures were found at the Hyogo-ken Nanbu Earthquake (17 January, 1995). In a design of structures, it was certificated that most of these accidents could not occur even though the same amount of static load acted on the structures. On the other hand, it is well known that fracture toughness decreases with increasing strain rate. Strain rate effect on fracture toughness was ignored on the design stage of the structures. Considering the strain rate effect on fracture toughness is necessary to evaluate the resisting ability on brittle fracture of steel structures. Authors [1] had shown that fracture toughness is the function of strain rate-temperature parameter (R) proposed by Bennet et al. [2] under arbitrary strain rate and temperature condition. The estimation method of fracture toughness under arbitrary strain rate and temperature by using the results of static fracture toughness test had also stated in ref.[1] in detail. Rparameter, which is derived from thermaly activated process of dislocation behaviour, is defined in Eqn. 1. R=T ln(A/˙ε) (1) where T: temperature [K], A: frequency factor (= 108[s−1]), ˙ε: strain rate [s−1]. In this study, an evaluation of brittle fracture accident occurred in the centrifugal cast steel bridge pier at the Hyogoken Nanbu Earthquake was performed by using the method in ref.[1]. An outline of the concept for
RkJQdWJsaXNoZXIy MjM0NDE=