the SEM micrographs of a typical primary carbide in the notch region of steels before and after its failure. Comparing the values of critical forces from Table 1, one may conclude that the failing force for the specimens with orientation LC is much higher than with the orientation CR (more than twice). Then, the force at which first microcracks form and first carbides fail depends on the orientation of specimens much more for high speed steels than for the cold work steels. a) b) Figure 3. A carbide grain before (a) and after failure (b). (Area size 40x100 µm). MESOMECHANICAL SIMULATION OF DEFORMATION IN STEELS To simulate the deformation of 3-point bending specimens with inclined notch, a threedimensional FE model of the specimen was developed. Due to the symmetry of the specimen, only one half of the specimen was taken. The material was assumed to be homogeneous. The forces measured in the tests described above were applied in the simulations. The displacements from the boundary nodes of elements which are located in the vicinity of the symmetry plane and at the lower notch boundary are used as boundary conditions in the mesomechanical simulation of carbide failure. Then, the 2D mesomechanical simulations of carbide failure have been carried out for each microstructure and each load, measured in the experiments. The 2D-model was created, which represents the cluster of finite elements in the notch region of the specimen. The real structure region with 5000 elements of the plane strain type TRIP 6 and size 100 µm x 100 µm was located in the lower left corner of the model. As boundary conditions the displacements from the model of deformation of 3-point bending specimen were taken. Since the mesh density in the 2D case is higher, the calculated displacements have been linearly interpolated between the points which were available in the 3D simulation. The mesomechanical simulation was performed with the use of the multiphase element method [5]. The micrograph of the carbide, obtained in SEM-in-situ experiments was digitized, and then automatically imposed on the region of the real structure. The micrographs to be digitized were chosen in such a way that they were representative enough for the given materials. Due to the inclined notch surface, the micrographs in Figure 3 have different scales in X- and Y-directions. To take that into account, the micrographs were scaled with the use of the image analysis software XView accordingly to their scales in both directions. The properties of carbide and matrix are as follows [3, 4, 6, 7]: (cold work steel) EC=276 GPa, EM=232 GPa, constitutive law of the matrix: σy = 1195 +1390 [1-exp (-εpl/0.0099)]; (high speed steels) EC=286 GPa, EM=231 GPa, constitutive law of the matrix: σy = 1500 + 471 [1exp(-εpl/0.0073)], Poisson's ratio - 0.19 (carbides) and 0.3 (matrix). 4

RkJQdWJsaXNoZXIy MjM0NDE=