areas in the vicinity of the lower boundary of the specimen; the local fluctuations of stresses caused by the carbides have evidently much more influence on the microcracking than the macroscopic stress field), and, finally, after the failure of many carbides, the microcracks (or plastic zones in front of the microcracks) begin to grow into the matrix; just after this occurs, the specimens fail. 2) The initial microcracks in the steels are formed in primary carbides (i.e. not along the carbide/matrix interface and not in the matrix). 3) The failing force for the specimens with orientation LC is much higher than with the orientation CR (more than twice). The force at which first microcracks form and first carbides fail depends on the orientation of specimens much more for high speed steels than for the cold work steels. 4) The failure stresses of carbides (of approximately average sizes for given steels) determined from the SEM in-situ experiments and the FEM simulations are 1826 MPa (the specimen KALC), 1840 MPa (KACR), 1604 MPa (HSCR) and 2520 MPa (HSLC). The failing stress of carbides depends of the orientation of carbide layers in high speed steels much more than in cold work steels. Acknowledgement: The authors gratefully acknowledge the financial support by the European Commission via the ECSC-Project 8834 ”Influence of micromechanical mechanisms on strength and damage of tool steels under static and cyclic loading”. The authors are grateful to the administration and specialists from the Technical University - Mining Academy Freiberg (TU BAF), who made it possible to carry out the SEM-in-situ experiments on their equipment and supported us during the experiments. References 1. L. Mishnaevsky Jr and S. Schmauder (2001), Appl. Mech. Rev, 54, 1 2. L. Mishnaevsky Jr, N. Lippmann and S. Schmauder (2000), In: Proc. 13th European Conference on Fracture “Fracture Mechanics : Applications and Challenges”, CD-ROM 3. L. Mishnaevsky Jr, N. Lippmann and S. Schmauder, Computational Optimization of Materials by Varying the Microstructures: Some Recent Developments as Applied to the Improvement of Fracture Resistance of Tool Steels (submitted) 4. N. Lippmann (1995), Dissertation, Freiberg, Germany 5. L. Mishnaevsky Jr, M. Dong, S. Hoenle and S. Schmauder (1999), Comp. Mater. Sci., 16, 1-4, 133-143 6. L. Mishnaevsky Jr and S. Schmauder, (2000), Influence of Micromechanical Mechanisms of Strength and Deformation of Tool Steels under Static and Cyclic Load, ECSC RTD Project Final Report, 2000, Creusot Loire, Frankreich 7. L. Mishnaevsky Jr and S. Schmauder (1999), Pursuance and Analysis of SEM-in-situ- Experiments on the Deformation and Fracture of Cold Work and High Speed Steels, MPA Report, 35 pp. 8. N. Lippmann, A. Lehmann, Th. Steinkopff and H.-J. Spies (1996), Comp. Mat. Sci., 7, 123-130 6
RkJQdWJsaXNoZXIy MjM0NDE=