MATERIAL AND EXPERIMENTAL PROCEDURES The material tested is a hot-isostatically sintered silicon nitride, Si3N4, developed by NGK Spark Plug Co. The density is measured as 3310 kg/m3. Fracture toughness (SEPB) and four point bending strength are 9.8 MPa m and 729 MPa, respectively. Rectangular bar specimen (3x4x40 mm) was subjected to four point bending with inner span of 10 mm and outer spans of 30 mm, at room temperature in air using hydraulic testing machine with load capacity of 10 kN. Figure 1(a) illustrates loading history of ∆P-increasing-type cyclic test. Stress ratio, R, of the cyclic loading is controlled as 0.1 and the cyclic loading frequency, f, is 20 Hz. Testing parameters of the ∆P-increasing test are the initial value, σmax,i, of maximum stress, σmax, and increasing rate of σmax, dσmax/dN(=2.8x10 -4 MPa/cycle). Provided that the value of σmax,i is sufficiently lower than σmax at failure, σmax,f, all the specimens tested are broken by cyclic loading, and the σmax,f value is evaluated for the individual specimens, as schematically illustrated in Fig. 2, where the effect of σmax,i is investigated. When the σmax,f values are analysed by Weibull distribution, fatigue strength can be evaluated statistically. Similarly, static fatigue strength can be evaluated by P-increasing test as illustrated in Fig. 1(b). Figure 3 shows AE monitoring system used. Two resonant-type AE sensors (Ch.1 and 2, PAC, PICO, center frequency of 0.58MHz) with a diameter of 4mm are mounted on the upper surface of the specimen opposite to the outer pins. Sensor outputs are amplified by a 40dB preamplifier and digitised by an A/D converter at a sampling interval of 50 ns with 1024 points at 10 bits. As the sensors monitor continuous noise with low frequency due to cyclic contacts of the specimen to two pins, trigger signal for AE events is prepared by using a new circuit. It has two functions of adding two sensor’s output and of filtering out the lower frequency components (-20 dB at 100kHz and -2 dB at 1 MHz). (b) (a) Figure1: Loading sequences of the (a)∆P-increasing test (cyclic fatigue) and (b)P-increasing test (static fatigue). Weibull probability Fracture stress σmax,f Effect of initial stress Maximum stress σmax d σmax/dt σmax,i Time t σmax,f 0 Figure.2: Schematic illustration of the ∆P-increasing tests and statistical analysis evaluating the effect of σmax,i on σmax,f.
RkJQdWJsaXNoZXIy MjM0NDE=