REFERENCE: ICF100497OR FIRST PRINCIPLES MOLECULAR DYNAMICS CALCULATION ON THE TENSILE STRENGTH OF Al GRAIN BOUNDARY Guang-Hong LU1, Masanori KOHYAMA2 and Ryoichi YAMAMOTO1 1 Institute of Industrial Science, University of Tokyo, 7-22-1 Roppongi, Minato-ku, Tokyo 106-8558, Japan 2 Department of Materials Physics, Osaka National Research Institute, AIST, 1-8-31 Midorigaoka, Ikedashi, Osaka 563-8577, Japan ABSTRACT The ab initio tensile test has been applied to Al Σ9(221)/[110] tilt grain boundary by first principles plane-wave pseudopotential method based on density functional theory with local density approximation. Stress-strain relation shows that the maximum stress of the Al Σ9 grain boundary is 9.9GPa at the strain of 28%. The changes of the charge density and the bond length indicate that the bonds at the boundary break first. KEYWORDS first principles, tensile strength, aluminum, grain boundary INTRODUCTION It is possible now to investigate the strength and mechanical behavior of defect, interface and grain boundary directly through first principles calculations on large supercell, using the first principles molecular dynamics method[1-3]. Deyirmenjian et al.[4] first performed ab initio tensile test on aluminum with atomic-scale void. Kohyama[5] performed the calculation of the tensile strength and fracture of a tilt grain boundary in
RkJQdWJsaXNoZXIy MjM0NDE=