CONCLUSIONS A finite element analysis was carried out for the failure behaviours of aligned fibre composites in terms of an embedded cohesive zone with matrix cracking and fibre-bridging. These two failure mechanisms, matrix cracking and fibre debond, pullout and fracture, are considered as separate entities, rather than under a single smeared-out bridging law. In describing the properties of fibre debonding and frictional sliding, a bi-linear constitutive law is used and in which, two parameters, η and , have been utilised to characterise these two effects on the fracture resistance. κ Numerical results show that the composite toughness can be increased by improving the interfacial properties. However, if the interface is too strong, low toughness can be caused by fibre breakage. Hence, high toughness can only be achieved by optimal design of the fibre-matrix interface. ACKNOWLEDGMENTS We would like to thank the Australian Research Council (ARC) for their continuing support of this project. H-YL acknowledges an ARC Postdoctoral Fellowship tenable at the University of Sydney. XZ was in receipt of an Overseas Postgraduate Research Studentship from the Australian Government and an ARC Scholarship from the research grant awarded to Y-WM. REFERENCES 1. Aveston, J., Copper, A. G. and Kelly, A. (1971) The properties of fibre composites. In Conference Proceedings, National Physical Laboratory, Guildford, 15-26. 2. Marshall, D. B. and Cox, B. N. (1985) Tensile fracture of brittle matrix composites, influence of fibre strength. Acta Metall. 35, 2607-2619. 3. Zhou, L.-M., Kim, J.-K. and Mai, Y.-W., (1992) On the single fibre pullout problem: effect of loading methods. Composite Science and Technology 45, 153-160. 4. Meda, G. and Steif, P. S. (1994) A detailed analysis of crack bridged by fibres. I: limiting cases of short and long cracks, J. Mech. Phys. Solids 42, 1293-1321. 5. Xia, Z. C., Hutchinson, J. W., Evans, A. G., and Budiansky, B. (1994) On large scale sliding in fibre-reinforced composites, J. Mech. Phys. Solids 42, 1139-1158. 6. Liu, H.-Y., Zhou, L.-M. and Mai, Y.-W., (1994) On fibre pullout with a rough interface. Philosophical Magazine A 70, 359-372. 7. Cox, B. N. and Marshall, D. B. (1994) Concepts for bridged cracks in fracture and fatigue, Acta Metall. Mater. 42, 341-363. 8. Zhang, X, Liu, H-Y, Mai, Y-W and Diao, X-X (1999) On steady-state fiber pull-out. Part I: stress field, Composite Science and Technology, 59, pp.2179-2189. 9. Liu, H-Y, Zhang, X, Mai, Y-W and Diao, X-X (1999) On steady-state fiber pull-out. Part II: numerical results, Composite Science and Technology, 59, pp.2191-2199. 10. Xu, G., Bower, A. and Ortiz, M. (1998) The influence of crack trapping on the toughness of fiber reinforced composites, J. Mech. Phys. Solids 46, 1815-1833. 11. Zhang, X, “Some Problems Relevant to Crack Propagation in Non-linear Solids”, PhD thesis, The University of Sydney, 1999. 12. Zhou, S. J. and Curtin, W. A. (1995) Failure of fiber composites: a lattice Green function model, Acta Metall. Mater. 43, 3093-3104. 13. Landis, C.M., Beyerlein, I. J. and McMeeking, R. M. (2000) Micromechaincal simulation of the failure of fiber reinforced composites, J. Mech. Phys. Solids 48, 621-648.

RkJQdWJsaXNoZXIy MjM0NDE=