A compact compression eccentrically loaded (CCEL) specimen for evaluating the fracture toughness of concrete has previously been reported by the author [6]. The test employs 100 mm concrete cubes modified by introducing two symmetrical notches on opposite faces and loaded eccentrically. The test provides the critical load at fracture, which is employed in a finite element analysis [7] to give the fracture toughness. The testing system was shown to be effective in identifying the differences in the toughness characteristics of concretes of different formulations [6]. The present study utilises this test to determine the fracture energy of concrete using two approaches, i.e. directly from the area under the load-displacement graph and indirectly from the stress intensity factor K. An alternative testing arrangement in which the specimen is loaded along the plane containing the two notches is also used to evaluate the fracture energy of the concretes employed. This test is referred to as the compact compression axially loaded (CCAL) specimen test. STRESS ANALYSIS Analyses of the two test geometries have been carried out using isoparametric finite elements [7,8]. Figure 1 gives the variations of the σy stress (normal to the crack plane) and the shear stress σxy along the plane containing the cracks for a unit applied load P on specimens with 30 mm symmetrical notches. The results demonstrate the rapid increase in the tensile σy stress along the ligament as the crack tips are approached. The absence of shear stresses along the ligament confirms that the fracture process is predominantly in the opening mode, which is evidenced in the actual tests. The fracture toughness Kc is directly related to the stress intensity factor K, which is obtained from the finite element analysis. The fracture toughness Kc is related to the critical value of the strain
RkJQdWJsaXNoZXIy MjM0NDE=