ICF10B

with a compressive strength of about 88 MPa. The Young’s modulus has been evaluated to be 38,000 N/mm2, while no information for unreinforced matrix fracture energy is available. Hooked-ends mild carbon steel fibers were used with average length of 60 mm, nominal diameter of 0.8 mm, aspect ratio of 75, and yield strength of 1100 MPa, with a fiber content of 1.5 %. By supposing a matrix fracture toughness equal to 0.14 Nmm−3/2 for the present case, we obtain N (1) P =1.276, N (2) P =3.0928 and ˜wE c =600, having supposed wc=1/3 of the length of the fiber. In order to evaluate the load-deflection theoretical curves, the costitutive moment vs localized rotation [10] has been used as a nonlinear hinge placed in the middle of the free span of the four point linear elastic beam [15]. Fig. 3.c shows the relationship between the applied load P and the middle-span deflection δ. The thin curve represents the experimental result, while the thick curve represents the theoretical one. After the linear elastic portion, an hardening behaviour appears due to the yielding of the primary reinforcement and to the bridging action of the fibers. Then, a softening behaviour is evidenced, due to the brittle failure (vertical drop) of the secondary fibers. It can be noticed a very small difference between the two curves, and only in the final portion, when the primary reinforcement yields, an error of 5 % has been achieved. CONCLUSIONS The proposed model represents an extension of the bridged crack model to the concurrent presence in a cementitious matrix of longitudinal bars and uniformly distributed fibers. A cohesive crack version can be obtained. It has been shown that the flexural behaviour of geometrically similar structures is governed by three dimensionless parameters. The influence of each parameter has been discussed in the proposed numerical examples, as well as an assessment between the curve predicted by the model and that obtained from an experimental test has been presented. This last result seems very promising for the consistency of the model. The model reproduces the structural behaviour of high-performance and/or fiber reinforced concrete members in bending. In particular, as the parameters are of easy physical meaning and of simple experimental evaluation, this model represents a very useful tool for the study of mechanical properties (strength and ductility) and of crack propagation regimes, according to concrete composition, typology and density of the fibers, distribution and characteristics of the longitudinal bars. A very important result of the theoretical formulation is provided by the dependence of the structural behaviour on the member size. Only with the same brittleness numbers it is possible to obtain physically similar structural responses. ACKNOWLEDGEMENTS The present research was carried out with the financial support of the Ministry of University and Scientific Research (MURST), the National Research Council (CNR) and the EC-TMR Contract No ERBFMRXCT960062. References 1. Barenblatt, G.I. (1962). In: Advances in Applied Mechanics, pp.55-129, Dryden, H.L., von Karman, T. (Eds.), Academic Press, New York. 2. Willis, J.R. (1967) J. Mech. Phys. Sol. 15, 151. 3. Rice, J.R. (1968) J. Appl. Mech. 35, 379. 4. Mashall,D.B. Cox, B.N. and Evans, G.A. (1985) Acta Metall. Mater. 33, 2013. 5. Rose, L.R.F (1987) Theor. Appl. Fract. Mech. 7, 125. 6. Jenq, Y.S. and Shah, S.P. (1985) J. Engng. Mech. 111, 1227. 7. Carpinteri, A. (1984) J. Struct. Engng. 110, 544. 8. Bosco, C. and Carpinteri, A. (1992) J. Engng. Mech. 118, 1564. 9. Carpinteri, A. and Massabo`, R. (1996) Int. J. Fract. 81, 125. 10. Carpinteri, A., Ferro, G. and Ventura, G. (2000). In: Composite Materials & Structures, pp.301-310, de Wilde, W.P., Blain, W.R., Brebbia, C.A. (Eds.). WIT Press, Southampton. 11. Okamura, H., Watanabe, K. and Takano, T. (1975) Eng. Fract. Mech. 7, 531. 12. Carpinteri, A. (1981) Mat. and Struct. 14, 151. 13. Carpinteri, A. and Massabo`, R. (1997) Int. J. Solids and Struct. 34, 2321. 14. Ashour, S.A. and Wafa, F.F. (1993) ACI Struct. J. 90, 279. 15. Carpinteri, A. and Massabo`, R. (1997) J. Engng. Mech. 123, 107.

RkJQdWJsaXNoZXIy MjM0NDE=