ICF10044OR FRACTURE MECHANISM OF A BAINITE STEEL IN PRECRACKED AND NOTCHED SPECIMENS AT LOW TEMPERATURE C. Yan1, J.H. Chen2 and Q. H. Qin1 1Centre for Advanced Materials Technology, School of Aerospace, Mechanical and Mechatronic Engineering, The University of Sydney, NSW2006, Australia 2Department of Materials Engineering, Gansu University of Technology, Lanzhou, Gansu, P.R. China ABSTRACT Precracked and notched specimens were used to investigate the fracture mechanism of a bainite steel at low temperature. The critical fracture event was studied using metallographic sectioning method. The results showed that the critical cleavage event was different in the precracked and the notched specimens. At -196oC, all specimens fractured at lower-shelf region without any ductile crack growth. The critical crack tip opening displacement was not sensitive to the depth of precrack. With increasing temperature to –100oC, cleavage was preceded by ductile crack growth for all precracked specimens. A longer ductile crack growth was associated with the shallow crack specimens, which resulted in a higher critical crack tip opening displacement. The ratio of depth to width of micro-dimple on ductile crack surface was decreased with ductile crack growth. KEYWORDS Fracture toughness, cleavage fracture, crack depth, ductile crack growth, bainite steel, fracture mechanism INTRODUCTION Previous research [1-3] showed that metallic materials, especially low-alloy high-strength (HSLA) steels had the different fracture mechanisms at low temperature in precracked and notched specimens. The work of Lin et al [2] in AISI 4340 steel showed that with increasing grain size there was an apparent improvement in fracture toughness (KIC) measured using precracked specimens but a decrease in Charpy V-notch impact energy. They attributed this to the variation of cleavage fracture stress and the characteristic distance over which the cleavage fracture can occur. Recently, the work of Chen et al on CMn steel [4-6] indicated that the cleavage fracture mechanisms were different in a precracked and a notched specimen. Currently, bainite steels have been increasing used in pressure vessels and piping industries due to superior weldability and fracture toughness. However, the fracture mechanisms of bainite steels are still not very clear. In this study, the fracture mechanism of a bainite steel was investigated using precracked and notched specimen at different temperatures. The cleavage fracture toughness and notch
RkJQdWJsaXNoZXIy MjM0NDE=